Rigid 10k solidified in the tank

Why would Rigid 10K solidify in a covered tank in a closed cabinet? The top layer was thick like play slime and discolored. The bottom resin in the tank was like taffy and stuck to the bottom (had to scrape it off to remove it). Was in the tank for maybe 45 days, way less than some of the other resins I have in tanks.

I don’t know I’m afraid but just from a knowledge point of view I suspect more details needed…

Temperature of storage (including swings)?
How long ago was it in good shape ?
How many prints? Any print failures?
When was it originally poured from the cartridge, expiry date of resin etc?