Hello Malissa
I also get mediocre results with my castings. (white, yellow or pink gold and silver)
Currently I have a open support ticket about this same issue.
I’m using plasticast with recommended times and temperatures without getting optimal results.
The last few times I’ve been increasing the time to get to 730º without substantial improvement…
Now i ordered a new resin bottle so that I can check if there are differences between lots.
On the other hand it would be interesting if someone who has solved this problem, described here the process and burnout cycle.
For my part if I can find the solution, I write it here
Regards