Fuse 1+ Speed Otimized problems

Dear Community,

Is there anyone who is using a Fuse1+ with PA12 Speed Otimized settings and getting good results?

Our specs:

  • PreForm 3.37.5.370
  • FW 1.18.2
  • 30% Material refresh
  • 32% packing density
  • Bed Temperature Offset now on -1.5C
  • Dosing offset -4.0 degree.

We are facing the following issues:

  • We are struggling with removing surface armour. Its bound so hard we are sweating to remove.
  • We have severe dimensional errors: 16mm nominal is rather 16.38mm. We done XY Scaling with legacy setting which could mess up a little but not that much I guess.
  • We have heavy amount of pitting and dimpling.
  • Heavy overdosing. The material spill is almost full under the linear track of the recoater and almost reaching the gears at the back.

Other than above the surface quality is superb.

If you have any advice on how should we get this thing dialed in? Should we use Default or Legacy instead and wait for Formlabs to fine tune that Speed Otimized setting?

Many thanks,

Mate

1 Like

Hi @snapfaab, thanks for your post. Sorry your having these issues!
We talked it over with a few of our SLS experts and agreed the best next step forward is to connect directly to our Customer Service team here. They’ll be able to help diagnose your problem in more detail and help you get flawless prints soon.

Hi, Thanks. We are debugging it now. Thanks!

1 Like