Long term warp of Form 3 parts

Just looking for some examples that I know exhibit warp and want to show how drying can affect warp. Basically will print a handful of parts, dry them at different amounts and then show the result. If you’re open to sharing the models and/or .form files, let me know!

I’d share if I had something

Dear leonhart88

I have read your blog.
I would appreciate if you could enlighten me on the following

It seems to me that underwater curing can save even more time than drying in a dryer.
Is there any difference in the effectiveness of secondary curing in water for different types of resins?
Is there any change depending on the water quality (pure water, ultrapure water)/water temperature?
After cleaning the molding with IPA, do you post-cure in water immediately after air-blowing the IPA? (Does it need to dry thoroughly before post-curing?) .
And, if we clean the molding before curing in water, is the standard time specified by FormLabs sufficient?