# Time saver easy depowdering of fuse and fuse 1+prints

**URL:** <https://forum.formlabs.com/t/time-saver-easy-depowdering-of-fuse-and-fuse-1-prints/44023>\
**Category:** Projects & Prints\
**Created:** [April 2, 2025, 1:08am UTC](https://forum.formlabs.com/t/time-saver-easy-depowdering-of-fuse-and-fuse-1-prints/44023 "2025-04-02T01:08:04Z")\
**Posts on this page:** 1\
**Showing post:** 38

<div class="post-metadata">

**Author:** ![mewertow](https://sea1.discourse-cdn.com/flex025/user_avatar/forum.formlabs.com/mewertow/32/22318_2.png) [@mewertow](https://forum.formlabs.com/u/mewertow)\
**Post date:** [April 30, 2025, 7:03pm UTC](https://forum.formlabs.com/t/time-saver-easy-depowdering-of-fuse-and-fuse-1-prints/44023/38 "2025-04-30T19:03:08Z")

</div>

Thanks! That does make sense - the vast majority of users run much lower PD. Anecdotally, air blasting like @MattRForerunner suggested can work well for certain types of parts if you really need more powder back faster - I’ve attached a chart below for a test build I ran where blue is manual time with a tool (brush), red is with air blasting. The other benefit is that air blasting should not remove the semi-sintered powder on your part, so you should be getting back only good powder.

@Mario_Martinez - I’m curious what your circumstance is as well. What typical packing densities / refresh rates do you run?