I’ve done a bunch of experimentation mixing resins. My goto is now 50% clear / 50% tough which I find is optimal for my prototype that relies extensively on precision waterproof silicone gasketed snapfit components. search around here for tuff and tufflex for a couple mixes I was testing.

---