# Laser Flare & the effects on your prints - Part II

**URL:** <https://forum.formlabs.com/t/laser-flare-the-effects-on-your-prints-part-ii/3716>\
**Category:** Support & Troubleshooting\
**Created:** [February 18, 2015, 11:28am UTC](https://forum.formlabs.com/t/laser-flare-the-effects-on-your-prints-part-ii/3716 "2015-02-18T11:28:17Z")\
**Posts on this page:** 1\
**Showing post:** 16

<div class="post-metadata">

**Author:** ![KevinHolmes](https://avatars.discourse-cdn.com/v4/letter/k/3ec8ea/32.png) [@KevinHolmes](https://forum.formlabs.com/u/KevinHolmes)\
**Post date:** [February 26, 2015, 3:51pm UTC](https://forum.formlabs.com/t/laser-flare-the-effects-on-your-prints-part-ii/3716/16 "2015-02-26T15:51:05Z")

</div>

@Steve_Johnstone so what’s the word from FL on a replacement machine?

Couldn’t tell from those shots, was there any porosity as well as the flaking?

My machine seems to be behaving very well now with the choke in place; flaking is pretty much gone, and I run prints at one higher exposure setting to make sure I don’t get porosity. That is - I set preform to print in clear when I actually have grey in the vat, black for clear, and so on. See @JoshK’s list of resin exposure times here [Resin list in order of exposure/curing?](http://forum.formlabs.com/t/resin-list-in-order-of-exposure-curing/3763).

Not only do I have almost no flaking, but surface slime also seems much reduced and requires less IPA brush scrubbing to remove. I even suspect small holes are more accurate; I just reprinted my glasses arms and they slotted on first try, whereas previously I was having to carve out gummy surface resin from the fixture slots with a scalpel.

![](http://forum.formlabs.com/uploads/formlabs/2749/1ab6000fcde1dbe1.jpg)

---

_[View the full topic](https://forum.formlabs.com/t/laser-flare-the-effects-on-your-prints-part-ii/3716)._