# IPA saturated with resin?

**URL:** <https://forum.formlabs.com/t/ipa-saturated-with-resin/2678>\
**Category:** General Discussion\
**Created:** [November 19, 2014, 12:24am UTC](https://forum.formlabs.com/t/ipa-saturated-with-resin/2678 "2014-11-19T00:24:54Z")\
**Posts on this page:** 2\
**Page:** 1

<div class="post-metadata">

**Author:** ![Tom\_Luhrs](https://avatars.discourse-cdn.com/v4/letter/t/ea666f/32.png) [@Tom\_Luhrs](https://forum.formlabs.com/u/Tom_Luhrs)\
**Post date:** [November 19, 2014, 12:24am UTC](https://forum.formlabs.com/t/ipa-saturated-with-resin/2678/1 "2014-11-19T00:24:54Z")

</div>

I print about 1L per month worth of parts and replace my IPA bath about that often as well. I soak my parts for 1 min then put the parts in IPA in an untrasonic cleaner for 5-10 min to remove uncured resin. Works great.

This time I went to dispose of the old IPA and found it swamped with what I assume is partially cured resin. Obviously not usable I am now curing the resin out but has anybody seen anything like this? Its like the IPA is saturated with resin but I have no idea where all this resin could have come from. Thanks.

![](http://forum.formlabs.com/uploads/formlabs/1294/83a951460bbd394b.JPG)

---

<div class="post-metadata">

**Author:** ![JasonSpiller](https://avatars.discourse-cdn.com/v4/letter/j/f14d63/32.png) [@JasonSpiller](https://forum.formlabs.com/u/JasonSpiller)\
**Post date:** [November 19, 2014, 2:08pm UTC](https://forum.formlabs.com/t/ipa-saturated-with-resin/2678/2 "2014-11-19T14:08:15Z")

</div>

I’ve had that gunge effect when either water is added or exposed to strong sunlight - as you surmise is just the resin in solution reacting. I filter my IPA using kitchen towel and 150 micron paint filter and it means I don’t have to replace the alcohol as often.