**Post date:** [November 21, 2020, 2:59am UTC](https://forum.formlabs.com/t/10k-resin/29408/1 "2020-11-21T02:59:48Z")

</div>

10k is easy to remove with fingernail. It is not as hard as sample sent of bottle opener.

Will heating it up to 105c fix this. Currently I did 70c 60 min

Is anyone sealing it with paint or finish of some kind

Thanks aloha

---

<div class="post-metadata">

**Author:** ![erikzweigle](https://avatars.discourse-cdn.com/v4/letter/e/ee59a6/32.png) [@erikzweigle](https://forum.formlabs.com/u/erikzweigle)\
**Post date:** [November 25, 2020, 12:27am UTC](https://forum.formlabs.com/t/10k-resin/29408/2 "2020-11-25T00:27:42Z")

</div>

Rigid 10k feels like a stick of chalk in my hand after curing for 60 min at 70°C. My pocket knife shaves imperfections off just as well as a file does. This part had minimal supports and the layer shift observed at the top of the sphere can be cleaned up with a fingernail as you mention. The sample part I received was a thick bottle opener with no thin walls so I hadn’t realized how brittle it was. The texture interested me enough to buy a liter since it was unlike any other thermoplastic I had worked with. The matte white color seemed like it would make a nice white Christmas ornament. For now I am just making trinkets. I can prime/paint it and let you know how it goes. Rigid 10k is very brittle. Dropping this 100mm spherical bauble from a height of 4 foot table and impacting an electrical power strip caused one of the beams to break.